Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 5.60 MPa
812 psi
ISO 527-3
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T..