Polymer Property : Film Tensile Strength at Yield, TD = 5323 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 36.70 MPa
5323 psi
ASTM D882
Honeywell Capran® NyLid™ WMB 250 Nylon Lidding Film  (discontinued **)
Description: Capran® NyLid™ WMB 250 is a 2.5 mil, white medium barrier nylon co-extruded film with an EVOH core. Applications: Capran® NyLid™ WMB 250 is suitable for die cutting, readily accepts..