Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 57.0 MPa
8270 psi
ASTM D882
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Film Tensile Strength at Yield, TD 57.0 MPa
8270 psi
ASTM D882
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..