Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 66.2 - 75.8 MPa
9600 - 11000 psi
ASTM D882
Honeywell Capran® Oxyshield™ OMBS (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Medium Barrier is a 0.60 mil (15 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug..
Film Tensile Strength at Yield, TD 66.2 - 75.8 MPa
9600 - 11000 psi
ASTM D882
Honeywell Capran® Oxyshield™ OMBS (1.00 mil) Monoaxially Oriented, Co-Extruded Nylon 6-Based Clear Film
Description: Oxyshieldâ„¢ Oriented Medium Barrier is a 1.00 mil (25 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug..