Polymer Property : Film Tensile Strength at Yield, TD = 667 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 4.60 MPa
667 psi
ISO 527-3
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch..