Polymer Property : Film Tensile Strength at Yield, TD = 7.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 7.10 MPa
1030 psi
ASTM D882
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and..
Film Tensile Strength at Yield, TD 7.10 MPa
1030 psi
at 2% offset; ASTM D882
ExxonMobil LD 307.76 Clear, High Impact Film Resin
LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical