Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 8.846 MPa
1283 psi
ASTM D882
Dow DOWLEX™ 2247G Polyethylene Resin
Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap..