Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 63.4 - 80.7 MPa | 9200 - 11700 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro.. |