Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 93.0 MPa
13500 psi
ASTM D828
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..