Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.175 g/micron
4.44 g/mil
ASTM D1922
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade  (discontinued **)
Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i..