Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.46 g/micron | 37.0 g/mil | Calculated from mfr's report of 0.8 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |