Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 10.8 g/micron | 275 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62030B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Elmendorf Tear Strength, MD | 10.8 g/micron | 275 g/mil | ASTM D1922 |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |
|||
Elmendorf Tear Strength, MD | 10.8 g/micron | 274 g/mil | |
Dow LDPE 526A Low Density Polyethylene, Blown Film Grade DOW LDPE 526A resin is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains medium levels of antiblock additive. .. |
|||
Elmendorf Tear Strength, MD | 10.8 g/micron | 274 g/mil | |
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Elmendorf Tear Strength, MD | 10.8 g/micron | 274 g/mil | |
Dow LDPE 752A Low Density Polyethylene, Film Grade DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu.. |