Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 13.7 g/micron | 348 g/mil | ASTM D1922 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Elmendorf Tear Strength, MD | 13.7 g/micron | 348 g/mil | |
Dow ATTANE™ 4213 Ultra Low Density Polyethylene ATTANE® 4213 copolymer is an ultra low density polyethylene that offers excellent flexibility, sealability, puncture resistance and superior strength. It exhibits oxygen transmission characteristic.. |
|||
Elmendorf Tear Strength, MD | 13.7 g/micron | 348 g/mil | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |