Polymer Property : Elmendorf Tear Strength, MD = 13.9 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 13.9 g/micron
353 g/mil
ASTM D1922
DuPont Surlyn® 1650SB
DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to ..