Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 6.34 g/micron | 161 g/mil | Calculated from mfr's report of 15.9 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |