Elmendorf Tear Strength, MD 6.50 g/micron
165 g/mil
ASTM D1922
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en..
Elmendorf Tear Strength, MD 6.50 g/micron
165 g/mil
ASTM D1922
ExxonMobil LD 051.LJ Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Elmendorf Tear Strength, MD 6.50 g/micron
165 g/mil
ASTM D1922
ExxonMobil LD 051.LT Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Elmendorf Tear Strength, MD 6.50 g/micron
165 g/mil
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade
DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl..
Elmendorf Tear Strength, MD 6.50 g/micron
165 g/mil
ASTM-D1922
Braskem TN2020 EVA General Film Copolymer
TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures..