Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.382 g/micron | 187.5 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness.. |