Polymer Property : Elmendorf Tear Strength, MD = 2.00 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin
Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu..
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11P2 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11P3 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11P4 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent sealing characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
Reliance Industries Reclair F18020 Polyethylene
Butene comonomer based Linear Low Density Polyethylene cast film grade. Reclair F18020 has optimum levels of antioxidants, and polymer processing aids. Applications:cast films, air bubble films, an..
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
Eastman Tritan MP100 Copolyester
Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co..
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM-D1922
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..
Elmendorf Tear Strength, MD 2.00 - 15.0 g/micron
50.8 - 381 g/mil
Average value: 7.72 g/micron Grade Count:11
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..