Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 2.17 g/micron | 55.1 g/mil | ASTM D1922 |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Elmendorf Tear Strength, MD | 2.17 g/micron | 55.0 g/mil | 1 mil; Cast Film; ASTM D1922 |
Chevron Phillips Marlex® HHM TR-166 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Elmendorf Tear Strength, MD | 2.17 g/micron | 55.0 g/mil | Calculated from mfr's report of 3.9 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 410 Paper, 7 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |