Polymer Property : Elmendorf Tear Strength, MD = 229 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 9.00 g/micron
229 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength..
Elmendorf Tear Strength, MD 9.00 g/micron
229 g/mil
ASTM D1922
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng..
Elmendorf Tear Strength, MD 9.00 g/micron
229 g/mil
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st..