Polymer Property : Elmendorf Tear Strength, MD = 24.5 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.965 g/micron
24.5 g/mil
ASTM D1922
LyondellBasell Alathon® L4434 High Density Polyethylene
ApplicationsALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches. Regulatory StatusL 4434 meet..