Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 10.6 g/micron | 269 g/mil | ASTM 1922 |
Braskem LQ 0518/30 LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; shrink film. Information provided by Braskem |