Polymer Property : Elmendorf Tear Strength, MD = 3.00 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.00 - 3.00 g/micron
25.4 - 76.2 g/mil
Average value: 1.86 g/micron Grade Count:7
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..