Elmendorf Tear Strength, MD >= 3.54 g/micron
>= 90.0 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 3.54 g/micron
90.0 g/mil
ASTM D1922
ExxonMobil EXACT™ 4151 Plastomer for Cast Film
Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer multilayer coextru..