Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 31.0 g/micron @Thickness 0.0250 mm |
787 g/mil @Thickness 0.000984 in |
ASTM D1922 |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |