Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.30 g/micron | 33.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Elmendorf Tear Strength, MD | 1.30 g/micron | 33.0 g/mil | |
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
Elmendorf Tear Strength, MD | 1.30 g/micron | 33.0 g/mil | ISO 6383-2 |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |