Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 32.8 - 39.4 g/micron | 833 - 1000 g/mil | |
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film
(discontinued **) Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc.. |