Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 15.4 g/micron | 390 g/mil | ASTM D1922 |
Dow ELITE™ 5401G Enhanced Polyethylene Resin ™ 5401G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking for excellent performance on a.. |
|||
Elmendorf Tear Strength, MD | 15.4 g/micron | 390 g/mil | Notched; ASTM D1922 |
Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Medium Antiblock, Processing Aid Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended w.. |