Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.87 g/micron
47.5 g/mil
Honeywell Stretch-Vac® 2000 Heat-Stabilized Blown Film  (discontinued **)
Description: Stretch-Vac® 2000 is a pink tinted, high elongation, heat-stabilized blown film produced from modified polyamide resin. It is available in widths up to 80 inches as layflat tubing and..
Elmendorf Tear Strength, MD 1.87 g/micron
47.5 g/mil
2 mil; ASTM D1922
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..