Elmendorf Tear Strength, MD 0.0217 - 1.87 g/micron
0.550 - 47.5 g/mil
Average value: 0.575 g/micron Grade Count:5
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..