Elmendorf Tear Strength, MD 18.80 g/micron
477.5 g/mil
ASTM D1922
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..