Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.90 g/micron
48.3 g/mil
ASTM D1922
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..