Polymer Property : Elmendorf Tear Strength, MD = 7.09 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 7.09 g/micron
180 g/mil
ASTM D1922
ExxonMobil LD 135.09 Cast Packaging Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging..
Elmendorf Tear Strength, MD 7.09 g/micron
180 g/mil
ASTM D1922
ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications
Product Description: Exact 3027 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3027 is designed for both monolayer and multilayer coe..
Elmendorf Tear Strength, MD 7.09 g/micron
180 g/mil
ASTM D1922
ExxonMobil LL 3201.22 Premium High Strength Film Resin  (discontinued **)
LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow..