Elmendorf Tear Strength, MD 7.20 g/micron
183 g/mil
ASTM-D1922
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene
TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness..