Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.20 g/micron | 208 g/mil | ISO 6383-2 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Elmendorf Tear Strength, MD | 8.20 g/micron | 208 g/mil | ASTM-D1922 |
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE .. |