Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.7106 g/micron | 221.25 g/mil | ASTM D1922 |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |