Polymer Property : Elmendorf Tear Strength, MD = 95.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD >= 3.74 g/micron
>= 95.0 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 3.74 g/micron
95.0 g/mil
ASTM D1922
Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin
Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform..
Elmendorf Tear Strength, MD 3.74 g/micron
95.0 g/mil
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film  (discontinued **)
Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as s..