Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 3.82 g/micron
97.0 g/mil
Average of MD and TD; ASTM D1922
DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film  (discontinued **)
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..