Elmendorf Tear Strength, TD 11.25 g/micron
285.8 g/mil
ASTM D1922
SCG Chemicals EL-Leneâ„¢ F15 High Density Polyethylene Film
Key Characteristics:High productivityHigh tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierExcellent printabilityRecommended Applications:High speed processingWide l..