Polymer Property : Elmendorf Tear Strength, TD = 14.27 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 14.27 g/micron
362.5 g/mil
ASTM D1922
ExxonMobil LL 3402.48 Cast Film Resin  (discontinued **)
LL 3402.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex..