Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 5.51 g/micron
140 g/mil
ASTM D1922
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness...
Elmendorf Tear Strength, TD 5.51 g/micron
140 g/mil
ASTM D1922
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness...