Polymer Property : Elmendorf Tear Strength, TD = 15.53 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 15.53 g/micron
394.5 g/mil
ASTM-D1922
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve..