Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 19.2 g/micron
488 g/mil
ASTM D1922
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b..
Elmendorf Tear Strength, TD 19.2 g/micron
488 g/mil
Dow AFFINITY™ PL 1850 Polyolefin Plastomer
AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc..