Polymer Property : Elmendorf Tear Strength, TD = 2.20 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process..
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim..
Elmendorf Tear Strength, TD 2.20 g/micron
55.9 g/mil
ASTM D1922-67
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used..
Elmendorf Tear Strength, TD 2.20 g/micron
55.9 g/mil
ASTM D1922
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
Dow 662I Low Density Polyethylene Resin
Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Elmendorf Tear Strength, TD 2.20 g/micron
55.9 g/mil
ASTM-D1922
Braskem F 7018 LDPE Extrusion Coating Polyethylene
LDPE F 7018 is a low-density polyethylene and has excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating; and injec..
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
Ashley Polymers Ashlene® 850 Nylon 6
This is an extrusion grade Nylon 6 resin suitable for both coextrusion and blown film applications. It has excellent melt stability and very high melt strength. It also has excellent grease resist..
Elmendorf Tear Strength, TD 2.20 - 7.00 g/micron
55.9 - 178 g/mil
Average value: 4.71 g/micron Grade Count:22
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..