Polymer Property : Elmendorf Tear Strength, TD = 22.93 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 22.93 g/micron
582.4 g/mil
ISO 6383/2
Borealis Borstar® FB4230 LLDPE for Film
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar ..