Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 24.951 g/micron
633.75 g/mil
ASTM D1922
Dow DOWLEX™ 2047G Linear Low Density Polyethylene
For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow