Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 0.984 g/micron | 25.0 g/mil | 1 mil; ASTM D1922 |
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide.. |
|||
Elmendorf Tear Strength, TD | 0.984 g/micron | 25.0 g/mil | Calculated from mfr's report of 2.5 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |