Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, TD = 25.4 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 1.00 g/micron
25.4 g/mil
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se..
Elmendorf Tear Strength, TD 1.00 g/micron
25.4 g/mil
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Elmendorf Tear Strength, TD 1.00 g/micron
25.4 g/mil
DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,..
Copyright © lookpolymers.com All Rights Reserved