Elmendorf Tear Strength, TD 11.0 g/micron
279 g/mil
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..