Polymer Property : Elmendorf Tear Strength, TD = 3.5665 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 3.5665 g/micron
90.589 g/mil
ISO 6383-2
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta..
Elmendorf Tear Strength, TD 3.5665 g/micron
90.589 g/mil
ISO 6383-2
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le..
Elmendorf Tear Strength, TD 3.5665 g/micron
90.589 g/mil
ISO 6383-2
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta..